this is my 2nd post and a question. u know the hard skin that forms on battery trminals. well i,m trying to dupicate that on cast lead bullets. i have been
soaking them in new battery acid and it kinda works, but it's not as hard
as the battery terminals. i would likw to speed up the process. maybe heat
needed, differant acid?? in my research, some plateing companys use
lead lined vats and the lead reacts with the acids and forms a skin and protects
itself. i do a lot of target shooting and bullets are expensive, so i cast my own.
i have 8 yrs pulp mill maintainance, clorine, caustic, clorates, and i make my own hot blueing salts from caustic soda and potasium nitrate. i hope someone
can help me with this. thanks Louis