TEMreplica Posted June 2, 2008 Posted June 2, 2008 When performing TEM on tissue samples, our group prepares a thin (1-2 microns) platinum replica to examine (2 mm in diameter). In this process, after spraying carbon for structural support, we dissolve the tissue from the replica by inserting it into bleach. When we remove the replica from the bleach and place it in DI water for cleansing, the surface tension of the water fractures it. Our group would greatly appreciate any advice to add avoid this fracturing. One idea we have is to use a mesh screening to add structural support. Another idea is to slowing drain the bleach from the petree dish until the replica sits on a soft, structurally strong surface. Then, add a dissolvable medium (maybe a gel) to add structural support upon entering the DI water. Lastly, drain the DI water slowly. Any thoughts are greatly appreciated.
DrP Posted June 2, 2008 Posted June 2, 2008 can the surface tension of the water be reduced with an additive (solvent or surfactant)? it might still need supporting but it may help reduce the stress a bit?
TEMreplica Posted June 3, 2008 Author Posted June 3, 2008 Yes, we have used an additive but it does not solve the problem completely. Thanks for the thought though.
Recommended Posts
Create an account or sign in to comment
You need to be a member in order to leave a comment
Create an account
Sign up for a new account in our community. It's easy!
Register a new accountSign in
Already have an account? Sign in here.
Sign In Now